Research paper
Experimental CharacterizationTheoretical| Type | Label | Value | Material | Sample | Condition | Source |
|---|---|---|---|---|---|---|
| Substrate Thickness | WSe₂ monolayer thickness | 0.8nm | — | |||
| Lateral Size | major diameter | 24.7nm | — | |||
| Lateral Size | minor diameter | 17.2nm | — | |||
| Rotation Angle | graphene/WSe₂ relative rotation angle | 26deg | — | |||
| Dirac Point Energy | off-GQD Dirac point | 0.12eV | — | |||
| Dirac Point Energy | on-GQD Dirac point | 0.4eV | — | |||
| Electrostatic Potential Parameter | betay | 6 | — | |||
| Electrostatic Potential Parameter | betax | 3.6 | — | |||
| Electrostatic Cutoff Radius | dy | 7.5nm | — | |||
| Electrostatic Cutoff Radius | dx | 4.5nm | — |
| Type | Label | Value | Material | Sample | Condition | Source |
|---|---|---|---|---|---|---|
| Substrate Thickness | WSe₂ monolayer thickness | 0.8nm | — | |||
| Lateral Size | major diameter | 24.7nm | — | |||
| Lateral Size | minor diameter | 17.2nm | — | |||
| Rotation Angle | graphene/WSe₂ relative rotation angle | 26deg | — | |||
| Dirac Point Energy | off-GQD Dirac point | 0.12eV | — | |||
| Dirac Point Energy | on-GQD Dirac point | 0.4eV | — | |||
| Electrostatic Potential Parameter | betay | 6 | — | |||
| Electrostatic Potential Parameter | betax | 3.6 | — | |||
| Electrostatic Cutoff Radius | dy | 7.5nm | — | |||
| Electrostatic Cutoff Radius | dx | 4.5nm | — |
| Type | Label | Value | Material | Sample | Condition | Source |
|---|---|---|---|---|---|---|
| Substrate Thickness | WSe₂ monolayer thickness | 0.8nm | — | |||
| Lateral Size | major diameter | 24.7nm | — | |||
| Lateral Size | minor diameter | 17.2nm | — | |||
| Rotation Angle | graphene/WSe₂ relative rotation angle | 26deg | — | |||
| Dirac Point Energy | off-GQD Dirac point | 0.12eV | — | |||
| Dirac Point Energy | on-GQD Dirac point | 0.4eV | — | |||
| Electrostatic Potential Parameter | betay | 6 | — | |||
| Electrostatic Potential Parameter | betax | 3.6 | — | |||
| Electrostatic Cutoff Radius | dy | 7.5nm | — | |||
| Electrostatic Cutoff Radius | dx | 4.5nm | — |
| Type | Label | Value | Material | Sample | Condition | Source |
|---|---|---|---|---|---|---|
| Substrate Thickness | WSe₂ monolayer thickness | 0.8nm | — | |||
| Lateral Size | major diameter | 24.7nm | — | |||
| Lateral Size | minor diameter | 17.2nm | — | |||
| Rotation Angle | graphene/WSe₂ relative rotation angle | 26deg | — | |||
| Dirac Point Energy | off-GQD Dirac point | 0.12eV | — | |||
| Dirac Point Energy | on-GQD Dirac point | 0.4eV | — | |||
| Electrostatic Potential Parameter | betay | 6 | — | |||
| Electrostatic Potential Parameter | betax | 3.6 | — | |||
| Electrostatic Cutoff Radius | dy | 7.5nm | — | |||
| Electrostatic Cutoff Radius | dx | 4.5nm | — |