Research paper
Experimental GrowthExperimental CharacterizationOther ComputationalEach sample groups how it was prepared, characterized, and measured. Click a card to expand.
5 preparations2 characterizations8 properties2 figures
5 preparations1 characterization1 figure
| Type | Label | Value | Material | Sample | Condition | Source |
|---|---|---|---|---|---|---|
| PL Peak | first excited state emission | 1150nm | — | |||
| PL Peak | ground state emission | 1210nm | — | |||
| PL Peak | cavity mode | 1160nm | — | |||
| Fet On Off Ratio | degree of circular polarization at cavity mode | 0.1 | — | |||
| Fet On Off Ratio | degree of circular polarization | negative in 1120-1230 nm range | — | |||
| Fet On Off Ratio | quality factor Q | 390 | — | |||
| PL Peak | simulated cavity transmission peak | 1176nm | — | |||
| Fet On Off Ratio | simulated cavity mode Q factor | 1167 | — |
Each sample groups how it was prepared, characterized, and measured. Click a card to expand.
5 preparations2 characterizations8 properties2 figures
5 preparations1 characterization1 figure
| Type | Label | Value | Material | Sample | Condition | Source |
|---|---|---|---|---|---|---|
| PL Peak | first excited state emission | 1150nm | — | |||
| PL Peak | ground state emission | 1210nm | — | |||
| PL Peak | cavity mode | 1160nm | — | |||
| Fet On Off Ratio | degree of circular polarization at cavity mode | 0.1 | — | |||
| Fet On Off Ratio | degree of circular polarization | negative in 1120-1230 nm range | — | |||
| Fet On Off Ratio | quality factor Q | 390 | — | |||
| PL Peak | simulated cavity transmission peak | 1176nm | — | |||
| Fet On Off Ratio | simulated cavity mode Q factor | 1167 | — |
Each sample groups how it was prepared, characterized, and measured. Click a card to expand.
5 preparations2 characterizations8 properties2 figures
5 preparations1 characterization1 figure
| Type | Label | Value | Material | Sample | Condition | Source |
|---|---|---|---|---|---|---|
| PL Peak | first excited state emission | 1150nm | — | |||
| PL Peak | ground state emission | 1210nm | — | |||
| PL Peak | cavity mode | 1160nm | — | |||
| Fet On Off Ratio | degree of circular polarization at cavity mode | 0.1 | — | |||
| Fet On Off Ratio | degree of circular polarization | negative in 1120-1230 nm range | — | |||
| Fet On Off Ratio | quality factor Q | 390 | — | |||
| PL Peak | simulated cavity transmission peak | 1176nm | — | |||
| Fet On Off Ratio | simulated cavity mode Q factor | 1167 | — |
Each sample groups how it was prepared, characterized, and measured. Click a card to expand.
5 preparations2 characterizations8 properties2 figures
5 preparations1 characterization1 figure
| Type | Label | Value | Material | Sample | Condition | Source |
|---|---|---|---|---|---|---|
| PL Peak | first excited state emission | 1150nm | — | |||
| PL Peak | ground state emission | 1210nm | — | |||
| PL Peak | cavity mode | 1160nm | — | |||
| Fet On Off Ratio | degree of circular polarization at cavity mode | 0.1 | — | |||
| Fet On Off Ratio | degree of circular polarization | negative in 1120-1230 nm range | — | |||
| Fet On Off Ratio | quality factor Q | 390 | — | |||
| PL Peak | simulated cavity transmission peak | 1176nm | — | |||
| Fet On Off Ratio | simulated cavity mode Q factor | 1167 | — |
figure_digitization.json#Figure 4(a)figure_digitization.json#Figure 4(sub)figure_digitization.json#Figure 5figure_digitization.json#Figure 4(a)figure_digitization.json#Figure 4(sub)figure_digitization.json#Figure 5figure_digitization.json#Figure 4(a)figure_digitization.json#Figure 4(sub)figure_digitization.json#Figure 5figure_digitization.json#Figure 4(a)figure_digitization.json#Figure 4(sub)figure_digitization.json#Figure 5